Patents and Publications
Patents
Mixture of Magnesite, Graphite, and Fine Particle Size Additive of Magnesium-Aluminum Alloy Coated with Magnesite, for Metallurgial Vessel Lining Bricks; Nonexplosive
|
Patent Number: 5,438,026 |
August 1, 1995 |
Indresco Inc. West Mifflin, PA 15122 Impact Sensor
|
Patent Number: 4,989,462 |
February 5, 1991 |
AGR International, Inc., Butler, PA 16001 Method and Apparatus for Testing Glassware
|
Patent Number: 4,733,973 |
March 29, 1988 |
AGR International, Inc., Butler, PA 16001 Method for Applying an Inorganic Coating to a Glass Surface
|
Patent Number: 4,261,722 |
April 14, 1981 |
AGR International, Inc., Butler, PA 16001 Method for Applying an Inorganic Titanium Coating to a Glass Surface
|
Patent Number: 3,926,604 |
December 16, 1975 |
AGR International, Inc., Butler, PA 16001 Publications
How Tin Oxide Coatings Affect Closure Rusting
|
Glass Worldwide |
2011 Fracture Analysis...Rely on Science, Not Guesswork
|
Glass Worldwide |
2011 Significance of Normalised Retardation Values in Stress Measurement
|
Glass Worldwide |
2010 Effects of Laser Coding on Glass Bottles and Its Effects on Performance of the Ware
|
Glass Worldwide |
2010 Glass Bottle Design and Performance
|
The Wiley Encyclopedia of Packaging Technology, 3rd Edition |
2009 Knowledge, the Key to Making Wise Decisions about Glass Container Performance and Problems
|
Glass Machinery Plants & Accessories |
2008 Practical Aspects of the Visco-elastic Behavior of Glass
|
Glass Machinery Plants & Accessories |
2008 Pressure Testing of Non-Pressure Ware
|
Glass Worldwide |
2007 AFM Analysis of Hot-end Coatings on Glass Containers
|
The Glass Researcher |
2000 Effect of Tin Oxide Coatings on Retardation Measurements of Cord Stresses in Glass Containers
|
Glass Industry |
2000 Effect of Lightweighting on the Impact Performance of Lightweight, Non-Round Glass Containers
|
International Glass Journal |
1999 Optimum Thickness Distribution for Lightweight Glass Containers
|
Glass Technology |
1995 Fracture of Glass Containers
|
Fractography of Glass, Edited by RC Bradt & RE Tressler |
1994 Bottle Strength Analysis
|
Glass |
1994 The Effect of Lightweighting on the Impact Performance of Glass Containers Further Discussions
|
Glass Technology |
1993 Recessed Label Panels - Another View
|
Glastechnische Ber. |
1993 Fracture Diagnosis Improves Quality and Performance
|
Glass |
1992 Surface-Energy Determinations of Tin Oxide-Coated Soda-Lime-Silica Glass
|
Journal of the American Ceramic Society |
1988 Thermally Induced Fast Fracture in a Glass Double-Cantilever Beam Specimen
|
Journal of the American Ceramic Society |
1988 Effects of Metal Oxide Coatings on the Strength of S-L-S Glass
|
American Ceramic Society Bulletin |
1987 Computer Modelled Internal Pressure Strength Predictions for Refillable Glass Containers
|
Glastechnische Ber. |
1986 The Characteristics of High-temperature Resistant Organic Polymers and the Feasibility of their Use as Glass Coating Materials
|
Journal of Materials Science |
1985 Interactions of Organic Coatings with Metal Oxide Coatings and Glass Surfaces
|
Glass Technology |
1985 A Super-Lightweight Container is Feasible (Originally Don't Say Can't)
|
Glass Industry |
1985 Optimization of the Glass Container Handling Process
|
Glass |
1985 Parameters Affecting the Deposition of Tin Oxide onto Glass Surfaces and the Function of Tin Oxide when Overcoated with Polythylene in Minimizing Glass Frictive Damage
|
Glastechnische Ber. |
1984 On the Static Fatigue Limit for Soda-Lime-Silica Glass
|
Glastechnische Ber. |
1983 A Critical Assessment of Lubricating and Damage Preventive Glass Coatings
|
Proceedings of the Third Toledo Glass and Ceramic Award Symposium, March 22, 1982 |
1982 Effects of Alkaline Solutions on Tin Oxide Coated Glass Surfaces
|
Glass Technology |
1981 The Mechanical Properties of Films for the Protection of Glass Surfaces
|
Thin Solid Films |
1981 Correlation Between the Electrical Resistivity of Tin Oxide Surface Coatings and their Microstructure
|
J. Non-Cryst. Solids |
1980 The Strength of Inorganic Glasses
|
Fundamental Phenomena in the Materials Science |
1967 Strength & Static Fatigue of Abraded Glass Under Controlled Ambient Conditions: IV, Effect of Surrounding Medium
|
Journal of the American Ceramic Society |
1961 The Effect of Chemical Composition on the Strength and Static Fatigue of Soda-Lime Glass
|
Physics and Chemistry of Glasses |
1961 Strength & Static Fatigue of Abraded Glass Under Controlled Ambient Conditions: III, Aging of Fresh Abrasions
|
Journal of the American Ceramic Society |
1960 Strength & Static Fatigue of Abraded Glass Under Controlled Ambient Conditions: I , General Concepts and Apparatus
|
Journal of the American Ceramic Society |
1959 Strength & Static Fatigue of Abraded Glass Under Controlled Ambient Conditions: II, Effect of Various Abrasions and the Universal Fatigue Curve
|
Journal of the American Ceramic Society |
1959 Cross-bending Tests of Glass Fibers and the Limiting Strength of Glass
|
Journal of Applied Physics |
1958